Theoretical and experimental study on the effect of stress corrosion on magnetic flux leakage signals
Author(s): |
Bingxun Zhao
Kai Yao Libo Wu Yufeng Fan Zhuang Sun Yue-Sheng Wang |
---|---|
Medium: | journal article |
Language(s): | English |
Published in: | Construction and Building Materials, October 2023, v. 399 |
Page(s): | 132461 |
DOI: | 10.1016/j.conbuildmat.2023.132461 |