Stress corrosion behavior of X80 pipeline steel in natural seawater with different dissolved oxygen

Author(s):

Medium: journal article
Language(s): English
Published in: Frattura ed Integrità Strutturale, , n. 50, v. 13
Page(s): 21-28
DOI: 10.3221/igf-esis.50.03
Structurae cannot make the full text of this publication available at this time. The full text can be accessed through the publisher via the DOI: 10.3221/igf-esis.50.03.