Optimization of Composition of Waterproofing Material Based on Modified Fine-Grained Concrete
Author(s): |
Aleksey Zhukov
Sofia Bazhenova Irina Stepina Irina Erofeeva |
---|---|
Medium: | journal article |
Language(s): | English |
Published in: | Buildings, 19 June 2024, n. 6, v. 14 |
Page(s): | 1748 |
DOI: | 10.3390/buildings14061748 |
Abstract: |
The purpose of the research described in this article was to optimize the compositions based on hydraulic-modified binder and construction waste for waterproofing and repair of concrete or brick structures in contact with the ground, as well as the study of properties and development of the basis of the methodology for selecting the composition of such a waterproofing system. Processing of the results of the experiment was carried out by statistical and analytical methods. The research was based on a method for determining the adhesive strength of a waterproofing coating, based on the determination when the insulating layers are torn off. As a result of the calculation and experimental verification, the composition of the waterproofing material was obtained, which corresponds to an adhesive strength of 3.8 MPa; the strength of the waterproofing layer was 36–37 MPa, as well as the amounts of the main components: acrylic resin 3.9%; finely ground concrete waste 80 kg/m3; plasticizer consumption (0.38…0.39%) at the optimum moisture content of the base surface (9.7…9.8%). |
Copyright: | © 2024 by the authors; licensee MDPI, Basel, Switzerland. |
License: | This creative work has been published under the Creative Commons Attribution 4.0 International (CC-BY 4.0) license which allows copying, and redistribution as well as adaptation of the original work provided appropriate credit is given to the original author and the conditions of the license are met. |