On the effect of weld defects on the fatigue strength of beam welded butt joints
Author(s): |
Ann-Christin Hesse
Thomas Nitschke-Pagel Klaus Dilger |
---|---|
Medium: | journal article |
Language(s): | English |
Published in: | Procedia Structural Integrity, 2018, v. 13 |
Page(s): | 2053-2058 |
DOI: | 10.1016/j.prostr.2018.12.209 |
- About this
data sheet - Reference-ID
10642496 - Published on:
10/01/2022 - Last updated on:
10/01/2022