Insight on the mechanical properties of hierarchical porous calcium-silicate-hydrate pastes according to the Ca/Si molar ratio using in-situ synchrotron X-ray scattering and nanoindentation test
Author(s): |
Sumin Im
Hyeonseok Jee Heongwon Suh Manabu Kanematsu Satoshi Morooka Hongbok Choe Nishio Yuhei Akihiko Machida JiHoon Kim Seungmin Lim Sungchul Bae |
---|---|
Medium: | journal article |
Language(s): | English |
Published in: | Construction and Building Materials, February 2023, v. 365 |
Page(s): | 130034 |
DOI: | 10.1016/j.conbuildmat.2022.130034 |