Enhanced hydration reaction of synthesized C4A0.81F1.19 with the use of different grinding agents

Author(s):


ORCID
Medium: journal article
Language(s): English
Published in: Materials and Structures, , n. 9, v. 57
DOI: 10.1617/s11527-024-02476-x
Abstract:

Tetracalcium aluminoferrite (C4AF) presents in ordinary Portland cement (OPC) as a solid solution phase, as C4AxF2−x (0.7 ≤ x ≤ 1.1). There is a limited understanding of the hydration reactions of C4AF, particularly regarding the influence of alkanolamines (AA) on C4AF, which can substantially alter OPC hydration. In this study, synthesized C4A0.81F1.19 was subjected to grinding, using three different AA (triisopropanolamine, ethanol diisopropanolamine, and diethanol isopropanolamine) at dosages of 0, 0.1, and 0.3%. It was experimentally confirmed that the crystal structure of unhydrated C4AF was partially changed during the grinding process, and the hydration properties of C4AF were modified. From these results, the compressive strength improved significantly, and the rate of strength enhancement was the highest with 0.1% of diethanol isopropanolamine. More specifically, it was revealed that both Fe and Al sources were proficiently activated, leading to the production of Al/Fe-containing AFm phases and efficiently enhanced mechanical properties.

Structurae cannot make the full text of this publication available at this time. The full text can be accessed through the publisher via the DOI: 10.1617/s11527-024-02476-x.
  • About this
    data sheet
  • Reference-ID
    10801993
  • Published on:
    10/11/2024
  • Last updated on:
    10/11/2024
 
Structurae cooperates with
International Association for Bridge and Structural Engineering (IABSE)
e-mosty Magazine
e-BrIM Magazine