Corrosion induced cover cracking studied by X-ray computed tomography, nanoindentation, and energy dispersive X-ray spectrometry (EDS)
Author(s): |
Branko Savija
Mladena Luković Seyed Amir Sajjad Hosseini José Pacheco Erik Schlangen |
---|---|
Medium: | journal article |
Language(s): | English |
Published in: | Materials and Structures, July 2015, n. 7, v. 48 |
Page(s): | 2043-2062 |
DOI: | 10.1617/s11527-014-0292-9 |
- About this
data sheet - Reference-ID
10170908 - Published on:
11/12/2018 - Last updated on:
11/12/2018