Apparent Quality and Service Performance Evaluation of SCFFC in Tunnel Secondary Lining

Author(s): ORCID
ORCID
ORCID
Medium: journal article
Language(s): English
Published in: Buildings, , n. 4, v. 12
Page(s): 479
DOI: 10.3390/buildings12040479
Abstract:

After removing the mold from the secondary lining concrete of a tunnel, problems such as honeycomb and hemp surface easily occur. To obtain self-compacting fair-faced concrete (SCFFC) that can meet strength requirements and effectively solve the above problems, this research prepared SCFFC with different mix proportions and performed slump expansion, slump, J-ring expansion and mechanical tests. Additionally, this research comprehensively analyzed the SCFFC based on fuzzy mathematics to study its apparent quality and service performance. This research aimed to solve problems such as uneven bubbles and poor bubble diameter in C30 SCFFC, through a combination of defoaming and air entraining by adding defoamer and air-entraining agent according to different proportions for compound treatment. The defoamer dosage was 0.5‰ of that of water reducer, and the air-entraining agent dosage was 0.1‰ of that of cement. The workability and clearance passability of the concrete were optimal. At the same time, the apparent holes in the SCFFC were small, as were their area and quantity. The distribution and apparent color of the SCFFC were uniform. Considering the factors affecting the service performance of concrete and after a comprehensive analysis of the samples’ weights, subjection degree, variability, stability, and strength index, this research found that the ratio for obtaining a C30 SCFFC material with the highest apparent quality and service performance was as follows: cement:machine-made sand:crushed dtone:fly-ash:water = 4:8.6:9.3:1:2.2. The water reducer comprised 1.0% of the total mass of the cementitious materials. The defoamer dosage was 0.5‰ of that of water reducer, and the dosage of air-entraining agent was 0.1‰ of that of cement.

Copyright: © 2022 by the authors; licensee MDPI, Basel, Switzerland.
License:

This creative work has been published under the Creative Commons Attribution 4.0 International (CC-BY 4.0) license which allows copying, and redistribution as well as adaptation of the original work provided appropriate credit is given to the original author and the conditions of the license are met.

  • About this
    data sheet
  • Reference-ID
    10664255
  • Published on:
    09/05/2022
  • Last updated on:
    01/06/2022
 
Structurae cooperates with
International Association for Bridge and Structural Engineering (IABSE)
e-mosty Magazine
e-BrIM Magazine