Apparent Quality and Service Performance Evaluation of SCFFC in Tunnel Secondary Lining

Auteur(s): ORCID
ORCID
ORCID
Médium: article de revue
Langue(s): anglais
Publié dans: Buildings, , n. 4, v. 12
Page(s): 479
DOI: 10.3390/buildings12040479
Abstrait:

After removing the mold from the secondary lining concrete of a tunnel, problems such as honeycomb and hemp surface easily occur. To obtain self-compacting fair-faced concrete (SCFFC) that can meet strength requirements and effectively solve the above problems, this research prepared SCFFC with different mix proportions and performed slump expansion, slump, J-ring expansion and mechanical tests. Additionally, this research comprehensively analyzed the SCFFC based on fuzzy mathematics to study its apparent quality and service performance. This research aimed to solve problems such as uneven bubbles and poor bubble diameter in C30 SCFFC, through a combination of defoaming and air entraining by adding defoamer and air-entraining agent according to different proportions for compound treatment. The defoamer dosage was 0.5‰ of that of water reducer, and the air-entraining agent dosage was 0.1‰ of that of cement. The workability and clearance passability of the concrete were optimal. At the same time, the apparent holes in the SCFFC were small, as were their area and quantity. The distribution and apparent color of the SCFFC were uniform. Considering the factors affecting the service performance of concrete and after a comprehensive analysis of the samples’ weights, subjection degree, variability, stability, and strength index, this research found that the ratio for obtaining a C30 SCFFC material with the highest apparent quality and service performance was as follows: cement:machine-made sand:crushed dtone:fly-ash:water = 4:8.6:9.3:1:2.2. The water reducer comprised 1.0% of the total mass of the cementitious materials. The defoamer dosage was 0.5‰ of that of water reducer, and the dosage of air-entraining agent was 0.1‰ of that of cement.

Copyright: © 2022 by the authors; licensee MDPI, Basel, Switzerland.
License:

Cette oeuvre a été publiée sous la license Creative Commons Attribution 4.0 (CC-BY 4.0). Il est autorisé de partager et adapter l'oeuvre tant que l'auteur est crédité et la license est indiquée (avec le lien ci-dessus). Vous devez aussi indiquer si des changements on été fait vis-à-vis de l'original.

  • Informations
    sur cette fiche
  • Reference-ID
    10664255
  • Publié(e) le:
    09.05.2022
  • Modifié(e) le:
    01.06.2022
 
Structurae coopère avec
International Association for Bridge and Structural Engineering (IABSE)
e-mosty Magazine
e-BrIM Magazine