Abrasion resistance behaviour of fly ash based geopolymer using nanoindentation and artificial neural network
Author(s): |
Chee Keong Lau
Hyuk Lee Vanissorn Vimonsatit Wai Yeong Huen Prinya Chindaprasirt |
---|---|
Medium: | journal article |
Language(s): | English |
Published in: | Construction and Building Materials, July 2019, v. 212 |
Page(s): | 635-644 |
DOI: | 10.1016/j.conbuildmat.2019.04.021 |