Experimental analysis of residual ultimate strength of stiffened panels with pitting corrosion under compression

Author(s):


Medium: journal article
Language(s): English
Published in: Engineering Structures, , v. 152
Page(s): 70-86
DOI: 10.1016/j.engstruct.2017.08.069
Structurae cannot make the full text of this publication available at this time. The full text can be accessed through the publisher via the DOI: 10.1016/j.engstruct.2017.08.069.