Experimental analysis of residual ultimate strength of stiffened panels with pitting corrosion under compression
Author(s): |
Jing Zhang
Xing Hua Shi C. Guedes Soares |
---|---|
Medium: | journal article |
Language(s): | English |
Published in: | Engineering Structures, December 2017, v. 152 |
Page(s): | 70-86 |
DOI: | 10.1016/j.engstruct.2017.08.069 |