Creep testing and analysis of recycled ceramic aggregate concrete-filled circle-shaped steel tube
Auteur(s): |
Hong Huang
Ao Wang Chao Yang Mengcheng Chen Yu Zhong Jinkai Chen Haiyang Zhuang |
---|---|
Médium: | article de revue |
Langue(s): | anglais |
Publié dans: | Construction and Building Materials, novembre 2024, v. 452 |
Page(s): | 138963 |
DOI: | 10.1016/j.conbuildmat.2024.138963 |