Ultimate strength of hybrid repaired offshore pipelines with various slenderness ratio subjected to through-thickness pitting corrosion under axial compressive loading

Author(s):


Medium: journal article
Language(s): English
Published in: Structures, , v. 60
Page(s): 105858
DOI: 10.1016/j.istruc.2024.105858