Systematic Rehabilitation Techniques and Dynamic Analysis of Bridge Deck System with Concrete-Filled Steel Tube Arches

Author(s):


Medium: journal article
Language(s): English
Published in: Buildings, , n. 12, v. 14
Page(s): 3891
DOI: 10.3390/buildings14123891
Abstract:

Due to prolonged heavy traffic, the Wuhan Changfeng Bridge has experienced extensive cracking in its main girder structure. Of the bridge’s 60 crossbeams, 51 (85%) have developed cracks, while the deck pavement over the steel beams has accumulated a total of 648.8 m of transverse cracks. Additionally, two T-beams exhibit structural vertical cracks of 0.3 mm at the mid-span, exceeding the maximum allowable width of 0.2 mm. This recurrent pavement damage not only compromises driving safety and comfort but also increases maintenance costs. To address these issues, this paper proposes a systematic upgrade plan for the bridge deck system. The plan involves welding additional high transverse beams onto the existing steel transverse beams, removing the original deck slab and replacing it entirely with an orthotropic steel deck. Additionally, two new steel longitudinal beams will be installed. The original simply supported concrete longitudinal beams in the deck will be transformed into an integrally connected continuous steel structure deck system. Using Midas/Civil finite element software, 3D models of Changfeng Bridge, pre and post renovation, were created to analyze the overall dynamic characteristics under five loading scenarios. The ambient vibration test and vehicle field test were conducted to measure the bridge’s natural frequency and impact factor, verifying the dynamic performance and driving comfort of the bridge after the upgrade. The results indicate that the retrofitted bridge experienced a 19.9% increase in overall stiffness. The dynamic performance of the bridge structure was significantly enhanced, and the most notable improvement was observed in dynamic stress, which decreased by 19.4% to 76.9%. Additionally, the steel deck reduced the bridge’s dead load, and the driving comfort on the bridge deck improved.

Copyright: © 2024 by the authors; licensee MDPI, Basel, Switzerland.
License:

This creative work has been published under the Creative Commons Attribution 4.0 International (CC-BY 4.0) license which allows copying, and redistribution as well as adaptation of the original work provided appropriate credit is given to the original author and the conditions of the license are met.

  • About this
    data sheet
  • Reference-ID
    10810607
  • Published on:
    17/01/2025
  • Last updated on:
    17/01/2025
 
Structurae cooperates with
International Association for Bridge and Structural Engineering (IABSE)
e-mosty Magazine
e-BrIM Magazine