Synergistic approach: Peridynamics and machine learning regression for efficient pitting corrosion simulation
Author(s): |
J. Ramesh Babu
S. Gopalakrishnan |
---|---|
Medium: | journal article |
Language(s): | English |
Published in: | Computers & Structures, December 2024, v. 305 |
Page(s): | 107588 |
DOI: | 10.1016/j.compstruc.2024.107588 |