Study on the influence of indentation depths on the fracture characterization and acoustic emission characteristics of minerals in granite using nanoindentation

Structurae cannot make the full text of this publication available at this time. The full text can be accessed through the publisher via the DOI: 10.1016/j.conbuildmat.2024.138516.