Study of the transition zone of concretes prepared with metakaolin using sem/eds-associated nanoindentation technique

Structurae cannot make the full text of this publication available at this time. The full text can be accessed through the publisher via the DOI: 10.1016/j.conbuildmat.2023.134717.