Quantitative fractography of fatigue cracks: a new solution in 3D
Author(s): |
Hynek Lauschmann
Karel Tesař Kateřina Jiroušková |
---|---|
Medium: | journal article |
Language(s): | English |
Published in: | Procedia Structural Integrity, 2019, v. 23 |
Page(s): | 107-112 |
DOI: | 10.1016/j.prostr.2020.01.071 |