Performance of Steel Beam-To-Column Connections with Weld Defects under Inelastic Cyclic Loading
Author(s): |
Binnur Goren Kiral
Secil Erim |
---|---|
Medium: | journal article |
Language(s): | English |
Published in: | Advances in Structural Engineering, August 2006, n. 4, v. 9 |
Page(s): | 561-575 |
DOI: | 10.1260/136943306778812804 |