Overload retardation effects on stress corrosion behaviour of prestressing steel
Author(s): |
J. Toribio
A. M. Lancha |
---|---|
Medium: | journal article |
Language(s): | English |
Published in: | Construction and Building Materials, October 1996, n. 7, v. 10 |
Page(s): | 501-505 |
DOI: | 10.1016/0950-0618(96)00015-3 |