Monitoring of thermoplastic induction welding defects. Use of electromagnetic properties as a predictive tool
Author(s): |
Mattia Mazzeschi
Karina C. Nuñez Esteban Cañibano Juan C. Merino (Foundation for Research and Development in Transport and Energy (CIDAUT), Spain) |
---|---|
Medium: | journal article |
Language(s): | English |
Published in: | Structural Health Monitoring, September 2022, n. 3, v. 22 |
Page(s): | 147592172211119 |
DOI: | 10.1177/14759217221111979 |