Investigation on Microstructure and Tensile Fractography of RE Oxides (CeO2/Y2O3) Reinforced AZ91D Magnesium Matrix Composites

Author(s): ORCID
ORCID
ORCID
Medium: journal article
Language(s): English
Published in: Frattura ed Integrità Strutturale, , n. 63, v. 17
Page(s): 100-109
DOI: 10.3221/igf-esis.63.10
Abstract:

The current work aims to investigate the mechanical properties of rare oxide reinforced Mg alloy based MMCs. Magnesium matrix considered in the study is AZ91D alloy, whereas rare earth oxides reinforced were CeO2 and Y2O3. The Y2O3 particulate reinforcement percentage was varied from 1 to 3% in the steps of 1% to study its influence on mechanical properties of MMCs. Stir casting route was adopted to fabricate sample for study. Microstructure analysis illustrated the uniform distribution of particulate in matrix alloys. The obtained results revealed the enhanced mechanical properties such as tensile strength, yield strength, elongation and hardness of MMCs due to increased percentage of reinforcement. Fractography analysis of fracture surfaces demonstrated the microcracks and cleavage were dominant in pure alloy. While particle debonding, extensive plastics deformation were prominent in-addition to microcracks in MMCs.

Structurae cannot make the full text of this publication available at this time. The full text can be accessed through the publisher via the DOI: 10.3221/igf-esis.63.10.
  • About this
    data sheet
  • Reference-ID
    10715843
  • Published on:
    21/03/2023
  • Last updated on:
    21/03/2023
 
Structurae cooperates with
International Association for Bridge and Structural Engineering (IABSE)
e-mosty Magazine
e-BrIM Magazine