0
  • DE
  • EN
  • FR
  • International Database and Gallery of Structures

Advertisement

The interfacial transition zone microstructure of ground ferronickel slag incorporated self-compacting concrete investigated by nanoindentation

Author(s): ORCID


Medium: journal article
Language(s): English
Published in: Journal of Building Engineering, , v. 71
Page(s): 106437
DOI: 10.1016/j.jobe.2023.106437
Structurae cannot make the full text of this publication available at this time. The full text can be accessed through the publisher via the DOI: 10.1016/j.jobe.2023.106437.