Improvement of Wetting and Bonding of Si02 Ceramics and Urea-Urethane Elastomer / Verbesserung der Benetzung und der Haftung zwischen Si02 Keramik und Harnstoff Urethan Elastomeren
Author(s): |
A. Boczkowska
K. Konopka K. Babski M. Szafran K. J. Kurzydtowski |
---|---|
Medium: | journal article |
Language(s): | English |
Published in: | Restoration of Buildings and Monuments, June 2007, n. 3, v. 13 |
Page(s): | 199-206 |
DOI: | 10.1515/rbm-2007-6132 |