High Temperature Fatigue Properties of Boron-doped Superalloy B1914
Author(s): |
Ivo Šulák
Karel Hrbáček Karel Obrtlík |
---|---|
Medium: | journal article |
Language(s): | English |
Published in: | Procedia Structural Integrity, 2023, v. 43 |
Page(s): | 209-214 |
DOI: | 10.1016/j.prostr.2022.12.260 |