Galvanic Corrosion of Carbon and Steel in Aggressive Environments
Author(s): |
Mohammadreza Tavakkolizadeh
Hamid Saadatmanesh |
---|---|
Medium: | journal article |
Language(s): | English |
Published in: | Journal of Composites for Construction, August 2001, n. 3, v. 5 |
Page(s): | 200-210 |
DOI: | 10.1061/(asce)1090-0268(2001)5:3(200) |