Fatigue strength of PF-1 coil helium inlet with weld defects.
Author(s): |
A. G. Kazantsev
M. G. Kakhadze K. A. Soin I. Y. Rodin S. N. Nasluzov |
---|---|
Medium: | journal article |
Language(s): | English |
Published in: | Procedia Structural Integrity, 2016, v. 2 |
Page(s): | 3562-3568 |
DOI: | 10.1016/j.prostr.2016.06.444 |