Fatigue properties of B1914 superalloy at high temperatures
Author(s): |
Vít Horník
Stanislava Fintová Miroslav Šmíd Pavel Hutař Karel Hrbáček Ludvík Kunz |
---|---|
Medium: | journal article |
Language(s): | English |
Published in: | Procedia Structural Integrity, 2019, v. 23 |
Page(s): | 191-196 |
DOI: | 10.1016/j.prostr.2020.01.085 |