Fatigue Performance Of Repairing Welds And Residual Stress Relieving For Corner Weld With Weld Defects
Author(s): |
Koei Takena
(THE JAPAN SOCIETY OF CIVIL ENGINEERS)
Fumio Itoh (THE JAPAN SOCIETY OF CIVIL ENGINEERS) Hirosuke Shimokawa (THE JAPAN SOCIETY OF CIVIL ENGINEERS) Chitoshi Miki (THE JAPAN SOCIETY OF CIVIL ENGINEERS) |
---|---|
Medium: | journal article |
Language(s): | English |
Published in: | 土木学会論文集 (Doboku Gakkai rombunshū), April 1989, n. 404, v. 1989 |
Page(s): | 315-320 |
DOI: | 10.2208/jscej.1989.404_315 |
- About this
data sheet - Reference-ID
10616144 - Published on:
24/08/2021 - Last updated on:
24/08/2021