Failure threshold analysis of weathering steel composite beams subjected to stress corrosion

Author(s): ORCID


Medium: journal article
Language(s): English
Published in: Structures, , v. 70
Page(s): 107763
DOI: 10.1016/j.istruc.2024.107763
Structurae cannot make the full text of this publication available at this time. The full text can be accessed through the publisher via the DOI: 10.1016/j.istruc.2024.107763.