Evaluating Stress Corrosion Damage of Steel Wires as Bridge Cables Based on the Corrosion Surface
Author(s): |
Rou Li
Hao Wang Changqing Miao Zhijie Yuan Ya Ni |
---|---|
Medium: | journal article |
Language(s): | English |
Published in: | Journal of Materials in Civil Engineering (ASCE), June 2024, n. 6, v. 36 |
DOI: | 10.1061/jmcee7.mteng-17275 |