Estimation of microstructural compositions in the weld zone of structural steel using nanoindentation

Author(s):


Medium: journal article
Language(s): English
Published in: Journal of Constructional Steel Research, , v. 99
Page(s): 121-128
DOI: 10.1016/j.jcsr.2014.04.011
Structurae cannot make the full text of this publication available at this time. The full text can be accessed through the publisher via the DOI: 10.1016/j.jcsr.2014.04.011.