Effect of pitting corrosion on strength of web plates subjected to patch loading
Author(s): |
Tatsuro Nakai
Hisao Matsushita Norio Yamamoto |
---|---|
Medium: | journal article |
Language(s): | English |
Published in: | Thin-Walled Structures, January 2006, n. 1, v. 44 |
Page(s): | 10-19 |
DOI: | 10.1016/j.tws.2005.09.004 |