The Effect of GFRP Wrapping on Lateral Performance of Double Shear Lap Joints in Cross-Laminated Timber as a Part of Timber Bridges

Author(s): ORCID
ORCID
ORCID

Medium: journal article
Language(s): English
Published in: Buildings, , n. 10, v. 12
Page(s): 1678
DOI: 10.3390/buildings12101678
Abstract:

Timber elements, such as timber bridges, are exposed to heavy loads. Therefore, reinforcement might be useful. Due to a lack of wood supplies, poplar, a fast-growing tree, could be used to construct CLT (cross-laminated timber). The low density of fast-growing wood species directly impacts the mechanical properties of CLT. Therefore, in this study, a CLT panel was reinforced with GFRP (glass-fiber-reinforced polymer), and the lateral resistance of double shear lap joints in reinforced CLTs with 0-90-0° arrangements in two strength directions was investigated. Lag screws (Ø = 8 mm) at the end distances of 1 and 3 cm were employed for making the lateral test specimens. First, the effect of the number of GFRP layers on lateral resistance of the joints was investigated. The results revealed that, as the number of GFRP layers changed from one to three, the lateral resistance increased by 45.47%, and then, by four layers, it decreased by 1.3%. Since the joints with three layers of FRP had the highest strength, the effects of the end distance and the CLT panel strength directions on the lateral performance of the reinforced and non-reinforced specimens were investigated. The results indicated that the lateral resistance of reinforced CLTs with GFRP was about 26.5% more than the unreinforced ones. Moreover, CLTs in the major strength direction showed 4.2% more lateral resistance than those in the minor strength direction. Moreover, lag screws at the end distance of 3 cm had 60% more lateral resistance than those at the end distance of 1 cm. In terms of failure modes, bearing, shear, and net-tension modes were observed in the CLTs, while Is, IIIs, and IV modes were observed in the lag screws.

Copyright: © 2022 by the authors; licensee MDPI, Basel, Switzerland.
License:

This creative work has been published under the Creative Commons Attribution 4.0 International (CC-BY 4.0) license which allows copying, and redistribution as well as adaptation of the original work provided appropriate credit is given to the original author and the conditions of the license are met.

  • About this
    data sheet
  • Reference-ID
    10700149
  • Published on:
    11/12/2022
  • Last updated on:
    19/02/2023
 
Structurae cooperates with
International Association for Bridge and Structural Engineering (IABSE)
e-mosty Magazine
e-BrIM Magazine