Durability of Fly Ash Geopolymer Mortars in Nitric Acid–Effect of Alkali (Na2o) Content/ Geopolimerinio skiedinio, pagaminto naudojant lakiuosius pelenus, ilgaamžiškumas azoto rūgštyje: šarmų (na2o) kiekio poveikis