Determination of Optimum Ingredients for Phosphogypsum Composite Stability under Marine Conditions-Response Surface Analysis with Process Variables
Author(s): |
Tingzong Guo
(Dept. of Civil and Environmental Engineering, Louisiana State Univ., Baton Rouge, LA 70803.)
James P. Geaghan (Dept. of Experimental Statistics, Louisiana State Univ., Baton Rouge, LA 70803.) Kelly A. Rusch (Louisiana State Univ., Institute for Ecological Infrastructure Engineering, Engineering Lab Annex Building, Baton Rouge, LA 70803 (corresponding author).) |
---|---|
Medium: | journal article |
Language(s): | English |
Published in: | Journal of Environmental Engineering (ASCE), April 2003, n. 4, v. 129 |
Page(s): | 358-365 |
DOI: | 10.1061/(asce)0733-9372(2003)129:4(358) |