Determination of mechanical properties in SM490 steel weld zone using nanoindentation and FE analysis
Author(s): |
Thai-Hoan Pham
Seung-Eock Kim |
---|---|
Medium: | journal article |
Language(s): | English |
Published in: | Journal of Constructional Steel Research, November 2015, v. 114 |
Page(s): | 314-324 |
DOI: | 10.1016/j.jcsr.2015.08.014 |