Cyclic testing of beam-to-column connections with weld defects and assessment of safety of numerically modeled connections from brittle fracture
Author(s): |
Koji Azuma
Yoshiaki Kurobane Yuji Makino |
---|---|
Medium: | journal article |
Language(s): | English |
Published in: | Engineering Structures, December 2000, n. 12, v. 22 |
Page(s): | 1596-1608 |
DOI: | 10.1016/s0141-0296(99)00115-7 |