Cross-scale mechanical softening of Marcellus shale induced by CO2-water-rock interactions using nanoindentation and accurate grain-based modeling
Author(s): |
Yiwei Liu
Quansheng Liu Zhijun Wu Shimin Liu Yong Kang Xuhai Tang |
---|---|
Medium: | journal article |
Language(s): | English |
Published in: | Underground Space |
DOI: | 10.1016/j.undsp.2024.02.001 |