Combined compression-bending performance and design of CFST with localised pitting corrosion
Author(s): |
Gen Li
Chao Hou Luming Shen |
---|---|
Medium: | journal article |
Language(s): | English |
Published in: | Journal of Constructional Steel Research, May 2022, v. 192 |
Page(s): | 107247 |
DOI: | 10.1016/j.jcsr.2022.107247 |