Abstract:

The paper presents a description and results of a study focused on the applicability of the sclerometric method to the preliminary assessment of concrete quality in structures after fire. Due to the high thermal inertia, concrete has non-uniform properties in the heated element cross-section. The greatest reduction of concrete compressive strength occurs on the heated surface. When assessing a structure after a fire, it is particularly important to determine the thickness of the damaged external concrete layer. Reinforced concrete beams exposed to high temperature on one side (a one-way heat transfer in the cross-section) for 0 (unheated element), 60, 120, 180 and 240 minutes were examined. A significant decrease of the rebound number on the elements heated surface was observed, depending on the heating duration. The obtained values of the relative rebound number reduction were comparable to the values of relative compressive strength decrease (determined on the basis of temperature) of concrete situated 15 mm from the heated surface.

Structurae cannot make the full text of this publication available at this time. The full text can be accessed through the publisher via the DOI: 10.2478/ace-2018-0069.
  • About this
    data sheet
  • Reference-ID
    10476697
  • Published on:
    25/11/2020
  • Last updated on:
    25/11/2020
 
Structurae cooperates with
International Association for Bridge and Structural Engineering (IABSE)
e-mosty Magazine
e-BrIM Magazine