The viscoelastic behaviour of material phases in fired clay identified by means of grid nanoindentation
Auteur(s): |
Hawraa Kariem
Josef Füssl Thomas Kiefer Andreas Jäger Christian Hellmich |
---|---|
Médium: | article de revue |
Langue(s): | anglais |
Publié dans: | Construction and Building Materials, janvier 2020, v. 231 |
Page(s): | 117066 |
DOI: | 10.1016/j.conbuildmat.2019.117066 |