Quantitative monitoring of localized pitting corrosion in steel bars through a combined use of distributed optical fiber sensors and finite element analyses
Auteur(s): |
E. Chen
Y. X. Li S. S. Zhang |
---|---|
Médium: | article de revue |
Langue(s): | anglais |
Publié dans: | Construction and Building Materials, août 2024, v. 438 |
Page(s): | 136970 |
DOI: | 10.1016/j.conbuildmat.2024.136970 |