On the processes causing the alteration of cement-based materials while drying: Differential scanning calorimetry as a reliable tool for indirect microstructural analysis
Auteur(s): |
Dalia Bednarska
Alicja Wieczorek Witold Grymin Kalina Materak Marcin Koniorczyk |
---|---|
Médium: | article de revue |
Langue(s): | anglais |
Publié dans: | Journal of Building Engineering, novembre 2022, v. 59 |
Page(s): | 105073 |
DOI: | 10.1016/j.jobe.2022.105073 |
- Informations
sur cette fiche - Reference-ID
10686824 - Publié(e) le:
13.08.2022 - Modifié(e) le:
23.09.2022