On the processes causing the alteration of cement-based materials while drying: Differential scanning calorimetry as a reliable tool for indirect microstructural analysis
Author(s): |
Dalia Bednarska
Alicja Wieczorek Witold Grymin Kalina Materak Marcin Koniorczyk |
---|---|
Medium: | journal article |
Language(s): | English |
Published in: | Journal of Building Engineering, November 2022, v. 59 |
Page(s): | 105073 |
DOI: | 10.1016/j.jobe.2022.105073 |