Investigating the Calcination Temperature and Grinding Time of Calcined Clay on the Mechanical Properties and Durability of LC3 Concrete
Auteur(s): |
Sina Nasiri
Rahmat Madandoust Malek Mohammad Ranjbar |
---|---|
Médium: | article de revue |
Langue(s): | anglais |
Publié dans: | Infrastructures, 12 octobre 2023, n. 10, v. 8 |
Page(s): | 139 |
DOI: | 10.3390/infrastructures8100139 |
Abstrait: |
The impact of the calcination temperature and grinding time on the mechanical properties and durability of limestone-calcined clay concrete (LC3) is crucial. In this research, calcined clay was produced within the temperature range of 700 °C to 900 °C, and the grinding time varied from 15 to 120 min. This study examines compressive strength and chloride penetration resistance using the rapid chloride migration test on LC3 concrete over a period of 180 days. The findings reveal that clay calcined at 800 °C for 120 min exhibited the highest specific surface area compared to other calcined clays. Furthermore, the compressive strength of LC3 concrete incorporating clay calcined at 800 °C for 60 min surpassed that of other mixtures investigated. Additionally, the chloride diffusion coefficient of LC3 concrete with calcined clay prepared at 800 °C for 120 min was lower than other mixtures. |
Copyright: | © 2023 the Authors. Licensee MDPI, Basel, Switzerland. |
License: | Cette oeuvre a été publiée sous la license Creative Commons Attribution 4.0 (CC-BY 4.0). Il est autorisé de partager et adapter l'oeuvre tant que l'auteur est crédité et la license est indiquée (avec le lien ci-dessus). Vous devez aussi indiquer si des changements on été fait vis-à-vis de l'original. |
5.63 MB
- Informations
sur cette fiche - Reference-ID
10746043 - Publié(e) le:
28.10.2023 - Modifié(e) le:
07.02.2024