0
  • DE
  • EN
  • FR
  • Base de données et galerie internationale d'ouvrages d'art et du génie civil

Publicité

Behavior of Orthotropic Steel-UHPC Composite Bridge Deck under Cyclic Loading

 Behavior of Orthotropic Steel-UHPC Composite Bridge Deck under Cyclic Loading
Auteur(s): , ,
Présenté pendant IABSE Symposium: Challenges for Existing and Oncoming Structures, Prague, Czech Republic, 25-27 May 2022, publié dans , pp. 810-819
DOI: 10.2749/prague.2022.0810
Prix: € 25,00 incl. TVA pour document PDF  
AJOUTER AU PANIER
Télécharger l'aperçu (fichier PDF) 0.14 MB

In recent years, ultra-high performance concrete (UHPC) has been introduced in the design of orthotropic steel decks (OSD) to reduce the risk of fatigue cracking. To investigate the fatigue behavio...
Lire plus

Détails bibliographiques

Auteur(s): (Department of Bridge Engineering, Tongji University, Shanghai, China; Department of Engineering Structures, Delft University of Technology, Delft, The Netherlands)
(Department of Bridge Engineering, Tongji University, Shanghai, China)
(Department of Engineering Structures, Delft University of Technology, Delft, The Netherlands m.veljkovic@tudelft.nl)
Médium: papier de conférence
Langue(s): anglais
Conférence: IABSE Symposium: Challenges for Existing and Oncoming Structures, Prague, Czech Republic, 25-27 May 2022
Publié dans:
Page(s): 810-819 Nombre total de pages (du PDF): 10
Page(s): 810-819
Nombre total de pages (du PDF): 10
DOI: 10.2749/prague.2022.0810
Abstrait:

In recent years, ultra-high performance concrete (UHPC) has been introduced in the design of orthotropic steel decks (OSD) to reduce the risk of fatigue cracking. To investigate the fatigue behaviour and fatigue damage process of the orthotropic steel-UHPC composite bridge deck, a full- scale specimen was designed and tested under cyclic loading. Test results show that the fatigue resistance of orthotropic steel-UHPC composite bridge deck satisfies the requirements of the designed vehicle load up to 2 million cycles with no cracks occurred in this phase. Rib-to-crossbeam weld and U-rib butt-welded connection are the two most vulnerable details to crack in OSD under cyclic loading. The fatigue resistance of U-rib bolted connection was investigated, and it is concluded that it performs better than that of U-rib butt-welded connection. The short-headed studs fractured under excessive cyclic loading and 5 types of the fatigue failure modes are identified. And the UHPC layer above the crossbeam exhibited limited number of cracks with the maximum crack width less than 0.05mm at the end of the cyclic, much beyond the requirements.

Mots-clé:
mouillages
Copyright: © 2022 International Association for Bridge and Structural Engineering (IABSE)
License:

Cette oeuvre ne peut être utilisée sans la permission de l'auteur ou détenteur des droits.