Understanding the field performance of asphalt binders in continental climates through modulated differential scanning calorimetry
Auteur(s): |
Justin Sandrasagra
Jianmin Ma Simon A. M. Hesp |
---|---|
Médium: | article de revue |
Langue(s): | anglais |
Publié dans: | Construction and Building Materials, août 2023, v. 391 |
Page(s): | 131857 |
DOI: | 10.1016/j.conbuildmat.2023.131857 |