Abstrait: |
Objective: This study investigates the influence of high-temperature treatment on the deformation properties and structural deformation of recycled aggregate concrete (RAC) in response to potential fire hazards in the construction industry. Methods: Standard-cured 28-day RAC specimens were subjected to microwave heating at 300 °C and 600 °C, with subsequent uniaxial compression tests utilizing a WDW-2000 machine and a VIC 3D strain measurement system to analyze strain data through digital image correlation (DIC) technology. Results: After treatment at 300 °C, recycled aggregate concrete (RAC) demonstrated superior mechanical properties to fresh concrete aggregates. This enhancement may be attributed to the more robust siloxane bonds (Si-O-Si) in the recycled materials. Conversely, exposure to 600 °C intensified internal structural damage, notably lowering the material’s elastic modulus and peak stress. DIC analysis highlighted the correlation among temperature, volumetric strain, and crack development patterns, with more extensive cracking at 600 °C. Conclusions: Moderate-temperature treatment enhances RAC’s structure and deformation properties, while high-temperature treatment diminishes its performance. These findings provide valuable insights for assessing building safety post-fire and the application of RAC, emphasizing its suitability at moderate temperatures and risks at high temperatures. |
Copyright: | © 2024 by the authors; licensee MDPI, Basel, Switzerland. |
License: | Cette oeuvre a été publiée sous la license Creative Commons Attribution 4.0 (CC-BY 4.0). Il est autorisé de partager et adapter l'oeuvre tant que l'auteur est crédité et la license est indiquée (avec le lien ci-dessus). Vous devez aussi indiquer si des changements on été fait vis-à-vis de l'original. |